SKAPS TRANSNET HDPE GEONET TN 270

SKAPS TRANSNETTM geonet consists of SKAPS GeoNet made from HDPE resin.

PDF Version
Property Test Method Unit Required Value Qualifier
Thickness ASTM D 5199 mil 270±15 Range
Carbon Black ASTM D 4218 % 2 to 3 Range
Tensile Strength ASTM D 5035 lb/in 75 Minimum
Melt Flow ASTM D 12383 g/10 min 1 Maximum
Density ASTM D 1505 g/cm3 0.94 Minimum
Transmissivity1 ASTM D 4716 m2/sec 3x10-3 MARV2

Notes:

1. Transmissivity measured using water at 21 ± 2°C (70 ± 4°F) with a gradient of 0.1 and a confining pressure of 10000 psf between stainless steel plates after 15 minutes. Values may vary between individual labs.

2. MARV is statistically defined as mean minus two standard deviations and it is the value which is exceeded by 97.5% of all the test data.

3. Condition 190/2.16